FLAME RETARDANT PIQUE

Composition:  60 % modacrylic, 38 % cotton, 2 % carbon

Indantrene dyed ( cotton )

Weight : 215 gr/m2 ( ± 5 % )

Width : 170 cm

Standards : 

EN ISO 11612 A1B1C1

EN 1149 -1

 

EN ISO 3071:2008 Ph Value Of Aqueous Extract : 6,8

EN ISO 14362-1:2007 Determination of certain aromatic amines derived from azo colorants : Not detected

EN ISO 3759:2011, EN ISO 5077:2008, EN ISO 6330:2012 Dimensional change after 5 washing cycles at 40 ◦C ) : Width : % -0,5 , Length : % -1

EN ISO 13938-1:2008 Bursting Resistance : 467 kPa

EN ISO 12947-2: 2017 Abrasion Resistance -Specimen breakdown with 9 kPa load , ( cycles ) : 8000

EN ISO 12945-2:2017 Surface fuzzing and pilling -modifiyed martindale method:

                Number of rubs            Grade

                           125                        4-5

                           500                        4-5

                           1000                      4-5

                           2000                      4-5

                           5000                        4

                           7000                        4

EN ISO 15025 Limited Flame spread (  After 5 washing cycles 40 ◦C ) : * No flaming to the top or either vertical edge,  * No hole formation in any direction,  * No flaming or molten debris, * No spreading afterglow on the undamaged area, * after flame time 0 s ,  * afterglow time 0 s                

EN ISO 9151:2016 Heat transmission on exposure to flame ( After 5 washing cycles 40 ◦C ) :  HTI24 : 4,8

EN ISO 6942:2003  ( metot B , pri 20 kW/m2 ) Heat transmission on exposure to radiant heat  ( After 5 washing cycles 40◦C  ) : RHTI24 : 14,3

EN 1149-1 Electrostatic properties surface resistivity, ( Ω ) After 5 washing cycles 40 ◦C ) : 5,7 * 108